Reinforced Concrete Beam Strength
Concrete takes the squeeze, steel takes the pull, and together they form a couple.
Before this Lesson
Squeeze 4,000 psi concrete, and it holds 4,000 psi. Pull on it, and it lets go at a few hundred. A loaded beam is squeezed along its top and stretched along its bottom, so a plain concrete beam cracks at the bottom, the crack runs straight up, and the beam breaks in two without warning.
So engineers put steel near the bottom, and then they do something that sounds like giving up: they let the concrete crack. Here's why that works, and how to put a number on what the beam can carry.
Let it crack
Load a beam that has steel bars near its bottom, and hairline cracks soon open along the bottom face. Each one climbs to the neutral axis, where stretching below turns into squashing above, and stops there. A crack can't pass a pull across itself, so below the neutral axis the steel carries all the tension. Above it, the concrete carries the compression.
That leaves a push in the concrete near the top and an equal pull in the steel. Two equal, opposite forces a distance apart make a couple, and the couple is the beam's moment: force times lever arm.
The Handbook's Design of Reinforced Concrete Components (ACI 318-14) section names the parts: , the width of the compression face; , the effective depth, from the extreme compression fiber to the centroid of the tension steel; , the area of that steel; , the concrete's strength from Concrete Strength and the Water-Cement Ratio; and , the steel's yield strength, usually 60,000 psi. And is the overall height.
The pull acts in the steel, so the lever arm starts there, and that's why strength uses , not . The cover below the bars keeps fire and corrosion away from them, but it sits on the cracked side and carries nothing.
What the concrete is doing when the beam fails
Keep loading. In a well-proportioned beam the steel yields first, so stops growing at . The beam keeps bending, the cracks climb, and the compression zone gets shallower and more squashed, until the top fiber reaches a strain of 0.003 and crushes. The moment then is the nominal moment strength, .
The strain grows in a straight line, from zero at the neutral axis, a depth below the top, to 0.003 at the top. The stress follows concrete's curved stress-strain curve, which is a nuisance to integrate. But the couple needs only two things from it: how big the push is, and where it acts. Charles Whitney swapped the curve for a rectangle that gets both right, which the Handbook calls the equivalent rectangular stress block: a uniform over a depth .
Source: Adapted from the FE Reference Handbook, Design of Reinforced Concrete Components (ACI 318-14), Internal Stress, Strain, and Forces due to Positive Moment Loading. Actual stress curve and labels added.
The Handbook's table gives 0.85 for up to 4,000 psi, then 0.05 less for each 1,000 psi above that, down to 0.65 from 8,000 psi up:
Stronger concrete has a more triangular stress curve, whose push sits higher, so the rectangle that matches it is shallower. The stress block rests on five assumptions, which the Handbook builds into its formulas without listing:
- Strain varies linearly with depth.
- The concrete crushes when the top fiber's strain reaches 0.003.
- The concrete carries no tension.
- The compression is a uniform over .
- The steel has yielded, so its stress is . This one gets checked.
The couple gives the strength
The steel pulls with , and the rectangle pushes with . They must balance, and that fixes :
The steel decides how big the force is, and the concrete only decides how deep the block reaches to supply it. acts at below the top, so the lever arm is :
The design strength is , with when the section passes the check in the next section, and the Handbook requires : demand versus capacity, .
The Handbook works in psi and in.-lb. Kips and inches work too and keep the numbers small, with in in.-kip divided by 12 for ft-kip. Just don't pair in psi with in ksi. comes from the Handbook's bar table:
| Bar size | Diameter (in.) | Area (in²) |
|---|---|---|
| #5 | 0.625 | 0.31 |
| #6 | 0.750 | 0.44 |
| #7 | 0.875 | 0.60 |
| #8 | 1.000 | 0.79 |
| #9 | 1.128 | 1.00 |
| #10 | 1.270 | 1.27 |
Source: Adapted from the FE Reference Handbook, Design of Reinforced Concrete Components (ACI 318-14), ASTM Standard Reinforcement Bars
Did the steel yield first?
The strain line can check the fifth assumption, and it tells you how much warning the beam gives. Since , the stress block gives . Carry the line down to the steel, and similar triangles give the net tensile strain:
The Handbook writes , the depth to the lowest layer of steel. With one layer, .
Grade 60 steel yields at about , with the 29,000 ksi the Handbook gives for steel. The Handbook's Resistance Factors table asks for more: only for a tension-controlled section, with . By the time the concrete crushes, that steel has stretched more than twice its yield strain, so the beam has cracked and sagged where everyone can see it. That warning is what rewards. Below 0.005, drops, as Designing Reinforced Concrete Beams shows.
For the worked example's beam, in., so , and holds. Add steel, and has to grow, so gets deeper. The line pivots on the 0.003 at the top, and less strain is left for the steel:
What makes a beam stronger
The steel sets the force, and sets the lever arm. The width and the concrete strength appear only as , inside , which reaches the lever arm only as . Here's the worked example's beam with one input doubled at a time:
| Doubled | (in.) | (ft-kip) | Change | |
|---|---|---|---|---|
| Nothing | 4.65 | 279.3 | none | 0.0080 |
| 9.29 | 485.2 | +74% | 0.0025 | |
| 4.65 | 595.3 | +113% | 0.0189 | |
| 2.32 | 297.6 | +7% | 0.0189 | |
| 2.32 | 297.6 | +7% | 0.0138 |
Doubling more than doubles , because the lever arm gains the full 20 in. while stays put. Doubling the steel falls short, because the block deepens and the arm shrinks, and drops below 0.005, so falls too. Doubling or only halves , which is worth 7%. The concrete just has to hold up its end of the couple, and a thin band across the top does that.
From strength to load
From Design Moments and Shears: a simple beam under a uniform load has at midspan, with , and checked in case the live load is small.
Set the demand equal to the capacity, and solve for the load:
That includes the beam's own weight, which comes from the whole section, by . The Handbook prints no unit weight for reinforced concrete, so a question gives one, usually 150 lb/ft³:
For the largest service live load, take out of , self-weight included, and divide what's left by 1.6.